Study on Preparation and Mechanical Properties of W-Cu Alloy with Low W-W Contiguity

  Electroless copper plating method combined with spark plasma sintering (SPS) was used to fabricate W-Cu alloy with low W-W contiguity.Results show that W-Cu alloy with low W-W contiguity and high relative density can be obtained by this method.With sintering temperature increased from 860℃ to 1060℃, the relative density of W-Cu alloy shows a rapidly increasing tendency, but the W-W contiguity keeps at a low level.Compression testing results show that the ductility of prepared W-Cu alloy is sensitive to strain rate, and the failure strain of the W-Cu alloy shows obviously increasing tendency with the loading strain rate increased from 10-3 to 103.

W-Cu alloy W-W contiguity Electroless plating Spark plasma sintering Mechanical properties

Hu Zhiyu Liu jinxu Li Shukui Qinghe Zou Wang Xing

Beijing Institute of Technology, Beijing 100081, China Mudanjiang North Alloy Tool Co., Ltd., Mudanjiang 157000, Peoples Republic of China Institute of Process Engineering, Chinese Academy of Sciences, Beijing 100190, China

国际会议

2014 SEM Fall Conference and International Symposium on Intensive Loading and Its Effects(国际实验力学学会2014年秋季会议、强化装载及其影响国际研讨会)

北京

英文

115-121

2014-10-19(万方平台首次上网日期,不代表论文的发表时间)