Thermal Decomposition Process of FeC2O4.2H2O in the Air
α-Fe2O3 nanoparticles are prepared at 550 ℃ by the thermal decomposition of FeC2O4.2H2O in the air.The morphologies of the pyrolysates of FeC2O4.2H2O in the air were investigated by scanning electron microscope (SEM).The results showed that in the process of the thermal decomposition of FeC2O4.2H2O, the influence on the pattern of the decomposition was more from 249.9 ℃ to 550 ℃.The influence on the pattern of the decomposition was less from 218.4 ℃ to 249.9 ℃.Therefore, the thermal condition of FeC2O4.2H2O in the air was controlled if the effective pattern of α-Fe2O3 powder was obtained.
FeC2O4.2H2O Thermal decomposition α-Fe2O3 nanoparticle
Zaizhi Yang Xiaoming Fu
The 3rd Department of Suqian College, Suqian Jiangsu 223800, P.R.China
国际会议
The Eighth China National Conference on Functional Materials and Applications(第八届中国功能材料及其应用学术会议)
哈尔滨
英文
135-138
2013-08-23(万方平台首次上网日期,不代表论文的发表时间)