The Synthesis and Solubility of a Wholly Aromatic Polyamide Containing para-and meta-Substituted Phenylene Rings
A series of wholly aromatic polyamides (aramid) containing para-and meta-substituted phenylene rings was eopolymerized via phosphorylation method with different ratio of 4-aminobenzoic acid and 3-aminobenzoic acid.The inherent viscosities (ηinh) of products were 0.52-0.99 dL/g.The chain structure of the polymers was characterized by Fourier transform infrared spectroscopy (FT-IR) and Raman spectrum.The differential scanning calorimetry (DSC) was also performed to investigate the chain transformation behavior of aramid.With increasing the content of meta-substituted phenylene rings in macromolecular chain, the solubility of the polymers was improved obviously without appreciable loss for their original thermal property.
Aromatic Polyamide Aramid Copolymerization Solubility
Yi-fan Wang Jun-Sun Li-xing Dai
College of Chemistry,Chemical Engineering and Materials Science,Soochow University,Suzhou 215123,China
国际会议
2012 China Functional Materials Technology and Industry Forum(2012中国功能材料科技与产业高层论坛)(CFMTIF2012)
昆明
英文
488-494
2012-11-09(万方平台首次上网日期,不代表论文的发表时间)