Hexavalent chromium leaching influenced factors in the weathering chrome slag

  The distribution of hexavalent chromium in the weathering slag was studied,as well as the influenced factors of aqueous agent leaching chromium.Results showed an optimal leaching condition:the chromium particle size is 100-200 mesh,the liquid-solid ratio is 20∶1,the leaching time is 4h 8h.Enhanced temperature and reduced pH value are benefit to hexavalent chromium leaching.Considering the equipment corrosion of low pH,the optimal pH value is 3-4.

weathering chromium slag hexavalent chromium leaching factors

Shuaixia Liu Liang Chen Yumei Gao

School of Environmental Science and Engineering, Donghua University, Shanghai 201602, China;Faculty School of Environmental Science and Engineering, Donghua University, Shanghai 201602, China Faculty of Material and Chemical Engineering, Henan Institute of Engineering, Zhengzhou 450007,China

国际会议

2013 International Symposium on Environmental Science and Technology(2013环境科学与技术国际会议)

大连

英文

629-632