  This study has investigated the degradation of H-acid (1-amino-8-naphthol-3,6-disulfonic acid) containing water by catalytic wet hydrogen peroxide oxidation method,in which the catalyst of Fe/SiO2 was prepared by impregnation technology.The effect of catalyst dosage,initial pH value,amount of hydrogen peroxide and reaction temperature on the degradation process have been discussed,and the results indicated that wet hydrogen peroxide oxidation is an effective method for treating the wastewater containing H-acid,under the conditions that:catalyst dosage was 2 g,initial pH value was 7,amount of hydrogen peroxide was 10 mL (0.83 time of theoretical required amount) and reaction temperature was 80 ℃,the COD and color removal rate can reach 87.3% and 96.5%,respectively.

Catalytic wet oxidation hydrogen peroxide Fe/SiO2 H-acid

Hongya Li Binxia Zhao Weili Bai Xiaoli Zhang

School of Chemistry and Chemical Engineering, Yulin University, Yulin 719000, China School of Chemical Engineering, Northwest University, Xian 710069, China Shaanxi Applied Physics and Chemistry Research Institute, Xi'an 710061, China

国际会议

2012 The 2nd International Conference on Biotechnology,Chemial and Materials Engineering(第二届生物、化工和材料工程国际会议(CBCME2012))

厦门

英文

281-284

2012-12-28(万方平台首次上网日期,不代表论文的发表时间)