Effect of hydrolysis on High-purity TiO2 Size for PTC Thermistor

  The effect of self-generated seeded thermal hydrolysis factors,such as TiOSO4 solution concentration,grey aging time,volume ratio of TiOSO4 to pre-adding water,and heating rate on high-purity TiO2 size for PTC thermistor were studied.The samples were characterized by particle size distribution,and SEM.The results show that with increase of TiOSO4 solution concentration,the high-purity TiO2 size decrease gradually,but with increase of grey aging time and volume ratio of TiOSO4 to pre-adding water respectively,the high-purity TiO2 size also increase.The suitable TiOSO4 concentration is 160g/l,grey aging time is 15min,the optimum volume ratio of TiOSO4 to pre-adding water is 4.0∶1 and heating rate should be 1.5℃/min.

high-purity TiO2 Hydrolysis Size

Zhiqiang Luo Jianqiao Du

PanGang Group Research Institute Co., Ltd., State Key Laboratory of Vanadium and Titanium Resources Comprehensive Utilization, Panzhihua, Sichuan, 617000, china

国际会议

the 2012 International Conference on Frontiers of Nanoscience and Technology(2012年纳米科学与技术国际会议(ICFNST 2012))

香港

英文

160-163

2012-07-26(万方平台首次上网日期,不代表论文的发表时间)