Solidification Simulation of Large Flat Ingot in different Intensive Cooling Conditions
The production of huge rectangular ingots becomes crying needs in the condition of lots of heavy plate mills more than 5m have been in operation.In this paper,we simulate the solidification of 60t Q235 huge rectangular ingot with ProCAST in different cooling conditions such as air cooling,forced air cooling and water cooling.The results show that solidification time in forced air cooling and water cooling shortened than that in air cooling respectively by 0.9 hours and 2.2 hours; The primary fine-grain area is large in the forced air cooling and water cooling.In forced air cooling,we can obtain the largest equiaxial crystal ratio and the minimum columnar crystal ratio; The shrinkage cavity position of the ingot in forced air cooling and water cooling is closer to riser than it is in air cooling,but the volumes of shrinkage cavities respectively increased to a greater extent than in air cooling.
Strengthening cooling Large flat ingot Solidification Simulation
Nan LV Shengli Li Yonglong jin Xingang Ai Dongwei zhang
University of Science and Technology Liaoning, Anshan, Liaoning, China Tangshan Iron and Steel Group Corporation, Tangshan, Hebei, China Anshan Iron and Steel Group Corporation, Anshan, Liaoning, China
国际会议
厦门
英文
517-520
2012-01-04(万方平台首次上网日期,不代表论文的发表时间)