会议专题

Mechanical Properties of Aerogel-Ceramic Fiber Composites

  Aerogel composites were prepared by immersing ceramic fiber into silica aerogel precursor via supercritical fluid drying.The mechanical behavior of silica aerogel composites was investigated with shrinkage,tension,bending and compression.The influences of fiber volume fraction,aerogel density and heat treatment were examined.After reinforced by ceramic fiber,the shrinkage of aerogel and aerogel-fiber composites was retarded obviously.The mechanical property of aerogel-fiber composites increased first and then decreased with increasing fiber volume fraction from 5.8% to 11.5%.For a given fiber volume fraction,the mechanical strength enhanced with increasing aerogel density.In addition,the mechanical property of aerogel composites did not decrease but increased after heat treatment at 600C.

Aerogel Mechanical property Fiber volume fraction

Gao Qing-fu Feng Jian Zhang Chang-rui Feng Jun-zong Wu Wei Jiang Yong-gang

State Key Laboratory of Advanced Ceramic Fibers & Composites, College of Aerospace and Materials Engineering, National University of Defense Technology, ChangSha 410073, China

国际会议

The Sixth China International Conference on High-Performance Ceramics(第六届中国先进陶瓷国际研讨会(CICC-6))

哈尔滨

英文

94-99