Preparation and Thermoelectric Properties of AgPb18SbTe20 Materials via Hydrothermal Synthesis Method
AgPb18SbTe20 nano-powders have been synthesized by a hydrothermal synthesis method at 180 ℃ for 20 h,using AgNO3,Pb(NO3)2,Sb(NO3)3,Na2TeO3 as starting materials and KBH4 as a reductant.AgPb18SbTe20 bulk thermoelectric materials were obtained by pressureless sintering at 450 ℃ or 520 ℃ under argon atmosphere,after uniaxial pressing the as-synthesized powders into pellets.The phase composition and thermal effects of as-prepared powders were characterized by X-ray diffraction (XRD) and DSC-TG analyses,respectively.Electrical properties of the as-prepared bulk materials were measured from room temperature to about 700 K,and the maximum power factor of 85 μW/mK2 was achieved at 600 K for the sample sintered at 723 K for 3 h.
AgPb18SbTe20 nano-powders Thermoelectric materials Hydrothermal synthesis
H.Li K.F.Cai H.F.Wang L.Wang X.L.Li
Functional Materials Research Laboratory,Tongji University,Shanghai 200092,P.R.China
国际会议
The Fifth China International Conference on High-Performance Ceramics (第五届先进陶瓷国际研讨会(CICC-5))
长沙
英文
550-552
2007-05-10(万方平台首次上网日期,不代表论文的发表时间)