Effect of Multiple Firing on Wear Behavior of Dental Veneering Ceramic

  This study investigated the effect of multiple firing on the wear behavior of dental all-ceramic veneering ceramic (Cercon).Samples were fabricated according to the manufacturers requirement for different firing times.The wear test was operated under simulated oral environment.The results showed that multiple firing could influence wear behavior of all-ceramic Veneer.Significant difference was observed in wear scar width among different samples.All the groups except 7time-firing one showed good wear resistance with low wear rate,smooth surface and relatively constant frictional coefficient.With the increasing firing times the wear scar width became larger.The wear resistance of dental ceramic after seven times firing was significantly lower.SEM/DFM results showed the wear facets of veneering ceramic demonstrate grooves characteristic of abrasive wear.The significant change was that severe wear dominated by brittle fracture could be seen in the 7time-firing group.Multiple firing can decrease the wear resistance of dental all-ceramic Veneer,and the wear pattern has the tendency to severe wear.The possible explanation is that the microstructure and properties of all-ceramic Veneering changed during multiple firing.

Wear Dental Ceramic Veneering Ceramic Multiple Firing

Q.P.Gao y.L.Chao F.Guo X.CH.Jian CH.J.Xu

Department of Prosthodontics,Xiangya Hospital,Central South University,Changsha 410008,China Department of Prosthodontics,West China College of Stomatology,Sichuan University,Chengdu 610041,Chi

国际会议

The Fifth China International Conference on High-Performance Ceramics (第五届先进陶瓷国际研讨会(CICC-5))

长沙

英文

1245-1247

2007-05-10(万方平台首次上网日期,不代表论文的发表时间)