On the Interface between Porcelain and Titanium
Low-fusing dental porcelain was fused on titanium surface.The adhesion between the titanium and porcelain was evaluated by three-point flexure test.It was shown that the failure of the titaniumporcelain predominantly occurred at the alloy-oxide interface.Rutile phase was present on the interface debonding from porcelain.The influence of corrosion on bonding strength was also investigated.The results suggested that,after being immersed in artificial saliva with pH of 2.7,5.4 and 7.0,no decreasing of the bonding strength of Ti-porcelain occurred.
Porcelain-fused-to-metal Titanium Three-point flexure test Corrosion
Litong Guo Jiqiang Gao Xiaochen Liu Tianwen Guo Zengying He
State Key Laboratory for Mechanical Behavior of Materials,Xian Jiaotong University,Xian 710049,P.R Department of Prosthodentics,Affiliated Hospital of Stomatology,School of Medicine,Zhejiang Universi The Fourth Military Medical University,Xian 710032,P.R.C
国际会议
The Fifth China International Conference on High-Performance Ceramics (第五届先进陶瓷国际研讨会(CICC-5))
长沙
英文
1618-1620
2007-05-10(万方平台首次上网日期,不代表论文的发表时间)