Synthesis of Bi0.5Sb1.5Te3/Graphene Composite Powders

  In this paper,Bi0.5Sb1.5Te3/graphene composite powders were prepared by hydrothermal synthesis method.X-ray diffraction (XRD),field emission scanning electron microscopy (FESEM) and transmission electron microscopy (TEM) were used to characterize the morphology and structure of the composite powders.As a nanocomposite phase,graphene provided plenty of charge carriers and active sites for nucleation of Bi0.5Sb1.5Te3 grains.Bi0.5Sb1.5Te3 particles aggregated and attached to the surfaces of graphene randomly.In addition,it was found that the sizes of Bi0.5Sb1.5Te3 particles varied with different content of graphene.The formation mechanism of Bi0.5Sb1.5Te3/graphene composite powders was discussed.

Graphene Bi0.5Sbl.5Te3 Thermoelectric materials

B.B. Liang Y. Li L.L. Xu L.J. Wang W. Jiang

State Key Laboratory for Modification of Chemical Fibers and Polymer Materials, Donghua University, 2999 North Renmin Road, Shanghai, 201620, China

国际会议

the Chinese Materials Congress 2012(2012年中国材料大会(CMC2012))

太原

英文

83-87

2012-07-13(万方平台首次上网日期,不代表论文的发表时间)