Influence of Titanium Sol on the Sintering Behaviour, Microstructure and Properties of Al2O3-SiO2 Ceramic Cores
A series of Al2O3-SiO2 ceramic cores with titanium sol sintered at 1350,1450,1500 and 1550℃for 2h,respectively,were prepared,and the phase and microstructure were characterized by X-ray Diffraction and Scanning Electron Microscopy.The influence of titanium sol on the phase transformation,shrinkage rate and flexural strength at room temperature has been investigated.The mullite phase formation temperature decreased by at least 150℃with the addition of 1wt% to 5wt% TiO2.Additionally,the titania additive promoted the combination of Al2O3 and SiO2,producing mullite phase which reduced the shrinkage and improved the flexural strength.
Ceramic core Al2O3-SiO2 Titanium sol Phase transformation Shrinkage Flexural strength
Jun Chen Yue Zhang
School of Materials Science and Engineering, Beihang University, Beijing 100191, China
国际会议
the Chinese Materials Congress 2012(2012年中国材料大会(CMC2012))
太原
英文
507-511
2012-07-13(万方平台首次上网日期,不代表论文的发表时间)