Effects of Roll Poreessing Rate and Heat Treatment on Microstuctures and Mechanical Properties of Ti75 Alloy Tube
The effects of deforming degree and annealling temperatures on performance of titanium alloy tubes Ti-75 are specified during 2-roller and multi-roller cold rolling process. The result shows that the alloy is sensitive for strain-hardening which has good cold processing performance by employing reduction 35%~40% for the cold rolling pass. The Ti75 alloy tube could obtain recrystallized structure with annealing at temperature 700~800t/1h/VC,and all quality and characteristic indications of thecold rolled products meet the requirement of technical standard.
Ti75 alloy deformation of cold rolling heat treatment
ZHAO Bin ZHAO Yong-qing YANG Ying-li GUO Di-zi Su Hang-biao WU Jin-ping
Northwest Institute for Nonferrous Metal Research,Xian 710016,China
国际会议
The 12th World Conference Titanium(第十二届世界钛会 Ti-2011)
北京
英文
314-317
2011-06-19(万方平台首次上网日期,不代表论文的发表时间)