Properties of Ti-5Al-4Mo-4V-4Cr-3Zr Titanium Alloy Bar
The mechanical properties of Ti-5Al-4Mo-4V-4Cr-3Zr bars with diameter of 16mm after heat treatment were investigated Results show that excellent strength and ductility could be achieved in Ti-5Al-4Mo-4V-4Cr-3Zr bars after solution treated blow beta transus plus aging treatment. There is a tendency that the tensile strength is increasing with the increase of solution temperatures on the same aging conditions. After solution plus aging treatment, the alloy can achieve the tensile strength within 1600 to 1400 MPa with the respective elongation of 8% to 14% and shear strength of 830 to 750MPa.
Beta titanium alloy solution plus aging strength ductility
GE Peng ZHOU Wei ZHAO Yongqing Wu Huan
Northwest Institute for Nonferrous Metal Research, Xian 710016, China
国际会议
The 12th World Conference Titanium(第十二届世界钛会 Ti-2011)
北京
英文
1141-1144
2011-06-19(万方平台首次上网日期,不代表论文的发表时间)