Fabrication and Characterization of Porous Ti by Powder Metallurgy

Porous Ti with the porosity range from 27. 3 to 30. 8 vol% were successfully fabricated by controlling sintering temperature. The morphology, pore structure and elemental composition were investigated by SEM and EDX. The results show that the characteristic parameters of porous titanium are controlled by sintering conditions.

Titanium (Ti) porous structure powder metallurgy

Guangzhong Li Huiping Tang Changshu Xiang Xinting Kang Wenyan Zhang Gang Li

State Key Laboratory of Porous Metal Materials, Northwest Institute for Non ferrous Metal Research, Xian 710076 ,China