Microstructure and Mechanical Properties of TiB and Ti-6Al-4V Composites by Powder-metallurgy

TiB-reinforced Ti-6A1-4V composites were fabricated by powder metallurgical processes from Ti,TiB2 and Al-V powders. The powders were mechanically blended in a high energy ball mill. The powder obtained was pressed into billets and sintered in vacuum atmosphere,then forging and other hot treatments were applied to improve the dispersion and size of TiB particles. SEM was used to study the influences of TiB particles in the composites on microstructure. Because of the formation of ultrafine and stable TiB reinforcements, the TiB reinforced Ti-6A1-4V composites are found to exhibit excellent mechanical properties at room temperature.

Titanium matrix composites (TMC) TiB microstructure mechanical properties

Yongren Liang Qingwen Duan Tuanwei Yang Yinjiang Wu

Xian Baode Powder Metallurgy Co. ,Ltd,Xian 710076 ,China Northwest Institute for Nonferrous Metal Research,Xian 710076,China

国际会议

The 12th World Conference Titanium(第十二届世界钛会 Ti-2011)

北京

英文

1523-1526

2011-06-19(万方平台首次上网日期,不代表论文的发表时间)