会议专题

The Synthesis and Characterization of Polyether-modified Polysiloxane Phosphate

In order to combine the properties of phosphate surfactants and silicone surfactants, the polyether-modified polysiloxane phosphate (PPSP) was prepared. Firstly, the intermediate was synthesized through the hydrosilylation of hydricpolysiloxane and alkyl polyether. Then the polyether-modified polysiloxane phosphate was prepared through the phosphorylation reaction of intermediate and P2O5. The optimum condition of the phosphorylation reaction was the reaction temperature was 80℃, reaction time was 3.5h and molar ratio of-OH: P2O5 was 3.0:1.0. The molecular structure of phosphate was characterized by FTIR and 31P-NMR. The components and their capabilities were also studied. The CMC of PPSP was 0.58g/L and the surface tension related was 25.78mN/m, but the foaming power of PPSP is relatively low.

Polyether-modified polysiloxane phosphate synthesis surface properties

Ren Longfang Wang Xuechuan Ding Jianhua

Key Laboratory of Aids Chemistry & Technology for Light Chemical Industry,Ministry of Education,Shaanxi University of Science & Technology,Shaanxi,Xian 710021,China

国际会议

2010 International Conference on Material and Manufacturing Technology(2010材料与制造技术国际会议 ICMMT2010)

重庆

英文

285-289

2010-09-17(万方平台首次上网日期,不代表论文的发表时间)