Glass wool prepared under various rotating speed by centrifugal-spinneret-blow process

In this paper, glass wool has been prepared under various rotating speed of centrifugal pan by centrifugal-spinneret-blow process. The fiber diameter of glass wool has been studied by scanning electron microscopy (SEM) and vertical optical microscope (VOM). With the increase of rotating speed from 1800 rpm to 2400 rpm, the mean fiber diameter decreased from 5.9 μm to 3.9 μm, indicating the distribution of glass wool becomes more uniformity. The results show that the rotating speed has a direct and pronounced effect on the fiber diameter and distribution. The higher the rotating speed is, the smaller the mean fiber diameter is, and the more uniformity the distribution of fiber diameter is.

Glass wool Rotating speed Centrifugal-spinneret-blow process

Bin Bin Li Zhao Feng Chen Zhou Chen Jin Lian Qiu Yan Qing Zhou Jie Ming Zhou

College of Material Science and technology, Nanjing University of Aeronautics and Astronautics,Nanji Suzhou VIP New Material Co., Ltd, Hong Da Fang Yuan Group, Suzhou, 215000, P.R. China

国际会议

2011 International Conference on Advanced Materials and Engineering Materials(2011先进材料与工程材料国际会议 ICAMEM 2011)

沈阳

英文

1573-1576

2011-11-22(万方平台首次上网日期,不代表论文的发表时间)