Quality Requirements for General Electric Ductile Iron Castings Exceeding 10T Used for Wind and Gas Turbine Components
Nodular Ductile Iron(NDI)components>10T for gas or wind turbines frequently utilizes either ASTM A395 or ENl563(EN-GJS-400-18U-LT)material.This paper reviews the actual cast components beyond external damage and m Jcroshr Jnkage,and focuses on darkened metal(chunky graphite)exposed by rough or finish machining(where the machined plane has intersected a solidification hot spot).Within the hot spot it will be shown that a chunky graphite morphological change has occurred.This will cause reductions in tensile and fatigue properties.Steps for identifying, investigating,and eliminating such indications are also discussed
nodular ductile iron chunky graphite dark spots wind turbines gas turbines low cycle fatigue UTS YS EL nodularity
G.K.Bouse J.Parolini N.Rojek C.Zhou
General Electric ENERGY,Materials & Protests Engineering,Grenville,SC,USA General Electric ENERGY,Materials & Protests Engineering,Warsaw,Poland General Electric ENERGY,Materials & Protests Engineering,Shanghai,China
国际会议
69th World Foundry Congress(第69届世界铸造会议 WFC 2010)
杭州
英文
889-893
2010-10-16(万方平台首次上网日期,不代表论文的发表时间)