The Wear Resistance of Pack-Boronizing of The Oilstone Forming Die
The main failure forms of oilstone forming die is serious wear on the work face, so the key point to extend the use life of die is how to control the wear, hi order to improve the hardness and resistance to wear and prolong the use life of the oilstone forming die, the boronizing technology was used on the work face of the oilstone forming die. There are some of elements such as B、 C、 Al、 Cr、 Si and Fe etc in boronizing layer, all of them change their contents during boronizing. Maximum value of microhardness of boronizing layer appears in subsurface, not in surface, and lows along depth of boronizing layer. The abrasion resistance of boronizing layer comes out maximum after quenching and tempering. After quenching and tempering, the lifetime of the oilstone forming die with boronizing is greatly improved.
Wear Resistance Oilstone Forming Die Pack-Boronizing Boronizing
Jing Chen Shaoxiang Hao Xun Fan
Departments of Mechanical Engineering,Henan Institue of Engineering. Zhengzhou, China School of Mech Departments of Mechanical Engineering,Henan Institue of Engineering. Zhengzhou, China School of Mechanical, Electronic and Information Engineering,China University of Mining & Technology
国际会议
2010 International Conference on Advanced Mechanical Engineering(2010年先进机械工程国际学术会议 AME 2010)
洛阳
英文
785-788
2010-09-04(万方平台首次上网日期,不代表论文的发表时间)