Influence of surface liquid segregation on corrosion behavior of semi-solid metal high pressure die cast aluminium alloys
The corrosion behavior (in chloride medium) of the surface layer of SSM-HPDC plates of alloys 7075-T6 and 2024-T6 was compared with that of the wrought alloys 7075-T6 and 2024-T6. Potentiodynamic testing was performed in deaerated 3.5%NaCl solution. In separate tests, the opencircuit potential was monitored in aerated 3.5% NaCI for 30 min after immersion. The electrochemical tests show that there is no significant difference in the pitting potential of the wrought alloys and that of the Cu-enriehed surfaces of the SSM-HPDC alloys.
semi-solid metal (SSM) forming wrought aluminium alloys alloy 7075 alloy 2024 corrosion surface liquid segregation
E.P.MASUKU H.M(O)LLER U.A.CURLE P.C.PISTORIUS W.LI
Materials Science and Manufacturing, Council for Scientific Industrial Research, Pretoria, South Afr Department of Materials Science and Engineering, Carnegie Mellon University, Pittsburgh, USA
国际会议
北京
英文
837-841
2010-09-16(万方平台首次上网日期,不代表论文的发表时间)