Selecting the Parameters for Brazing 08 Steel With Pure Copper Solder Paste

The larger variation of the construction and performance of the low-carbon steel joints was caused by the high temperature of the puddle welding of the joint. Therefore, the braze welding rather than the puddle welding was applied to the welding production of low-carbon steel. The 08 steel parts were joined in a furnace using pure copper solder paste as brazing filler metal. According to the obtained results, the ideal technical parameters are as follow: brazing temperature: 1100-1150℃; holding time: 5-10rain; joint clearance: 0.03-0.05mm.

Solder paste Brazing temperature Holding temperature Joint clearance

D.G.Chang J.Zhang M.L.Lv

College of Electromechanicel Engineering,Qingdao University of Science and Technology,Qingdao,Shando Chemical and Process engineering Department,University of Sheffield,Sheffield,Britain

国际会议

The 3rd Conference of Cross-Strait Engineering Education and Ceeusro & 1st International Conference on Engineering Technologies and Ceeusro(ICETC2009)(第三届工程技术与产学研研讨会暨第一届国际功能制造技术学术会议)

常州

英文

432-435

2009-11-19(万方平台首次上网日期,不代表论文的发表时间)