The thermal property of high performance fiber
High performance aramid fibers display their outstanding high tenacity, high modulus and high temperature resistant under various section. Kevlar129, PBO and Kennel fibers are compared for thermal properties. It can be found that the PBo fiber has the highest thermal degradation temperature by TGA in nitrogen atmosphere, and its initial degradation temperature is 556. 51.Accordingly, when heated under 100, 200,300,400℃ for 1.5h, the tenacity and the extension to break of Kev-Iar129, PBO and Kennel fiber all decrease with temperature, but the modulus increase firstly then decrease. PBo generally has higher mechanical property retention. From the SEM observation to these fibers treated under heat, the morphology show their fracture failure mode when they are tensiled, and there exists fibrils in their core.
Kevlar PBO Kermel thermal property degradation
LIU Xiao-yan TAO Yu-kun WANG Xiao-ling YU Wei-dong
College of Textiles, Donghua University, Shanghai 201620,China College of Textiles, Donghua University, Shanghai 201620,China College of Textiles and Materials, Wu
国际会议
2009 International Teztile Science and Technology Forum(2009国际纺织科学技术论坛)
西安
英文
267-271
2009-04-01(万方平台首次上网日期,不代表论文的发表时间)