会议专题

Effect of Y-doping on the piezoelectric properties of (1-z)BiScO3-zPbTiO3 high-temperature piezoelectric ceramics

(1-x)Bi(Sc1-yYy)O3-xPbTiO3 (BSYPTx/y) ceramics were prepared by the conventional mixed oxide method. It was found that the morphotropic phase boundary (MPB) between rhombohedral and tetragonal phase of BSYPTx/y system was moved to the lower PT content with increasing of BiYO3 content. The Curie temperature (TC) near MPB of BSYPTx/y ceramics was found to increase with increasing of BiYO3 content. However, the piezoelectric properties (d33 and kp) decreased with increasing of BiYO3 content. BSYPTx/y ceramics with x=0.56, y=0.2 showed a high TC of 490 ℃ and a large d33 of 147 pC/N.

piezoelectric high-curie temperature BSPT

Qishou Li Wei Shi Yuzhi Jiang Ying Pei Qiang Chen Xi Yue Dingquan Xiao Jianguo Zhu

College of Material Science and Engineering,Sichuan University,Chengdu,610064,China Surface Science College of Material Science and Engineering,Sichuan University,Chengdu,610064,China Department of Ph College of Material Science and Engineering,Sichuan University,Chengdu,610064,China

国际会议

2009 The 18th IEEE International Symposium on Applications of Ferroelectrics(2009年国际铁电学暨IEEE国际铁电应用联合会议)

西安

英文

382-385