Microstructure Analysis of AC Corona Aging of Silicone Rubber

A needle-plane electrode system was used to study the characteristics of the silicone rubber under AC corona. Microstructure and chemical structure change analysis on the surface of silicone rubber after corona ageing was made by using SEM, AFM and FTIR. Infrared spectrum shows that corona would cause the rupture of fundamental chain and branched chain of material. Along with the increase of corona aging time, the content of fundamental chain and branched chain will decrease. The continuous increase in the content of carbanyl group shows the intensifying oxidation. Hydroxyl -OH turns into combined condition from dissociative condition.

AC corona high-temperature vulcanized silicone rubber(HTV-SR) microstructure analysis SEM AFM FTIR

Congzhen XIE Yao ZHANG Jianguo WANG Yang Liu Yanpeng HAO Mingzhen GAO

School of Electric Power, South China University of Technology, Guangzhou Guangdong 510640,China School of Electrical Engineering, Wuhan University, Wuhan Hubei 430072, China Dongguan Power Supply Bureau,Dongguan Guangdong 523000, China

国际会议

第九届电介质材料性能与应用国际会议(The 9th International Conference on Properties and Applications of Dielectric Materials)

哈尔滨

英文

481-484

2009-07-19(万方平台首次上网日期,不代表论文的发表时间)