Preparation of Monodispersed Iron Nanoparticles by Thermal Decomposition
Monodispersed iron nanoparticles were prepared by thermal decomposition of iron carbonyl at low temperatures of 160-180 ℃ in kerosene. The iron nanoparticles were spherical and their average size was decreased from 11.2 nm to 8.6 nm with increasing decomposition temperatures in the range of 160 ℃ to 180 ℃. The as-prepared iron nanoparticles were amorphous, but the surface of the particles was easily oxidized to be spinel structured.
iron nanoparticle iron carbonyl thermal decomposition low temperature
SHAO Hui-ping LEE Hyo-Sook SUH Yong-Jae KIM Jong-Hee LI Ying KIM Chong-Oh
Department of Materials Science and Engineering, Chungnam National University, Daejeon 305-764, Kore Nano-materials Group, Korea Institute of Geoscience and Mineral Resources, Daejeon, 305-350, Korea Research Center for Advanced Magnetic Materials, Chungnam National University, Daejeon 305-764, Kore School of Materials Science and Engineering, Shanghai University, Shanghai, 200072 China
国际会议
北京
英文
205-208
2006-08-29(万方平台首次上网日期,不代表论文的发表时间)