Densification of Alumina Powder by Using PECS Process with Different Pulse Electric Current Waveforms
Densification and sample temperature of alumina (Al2O3) powder during pulsed electric current sintering with different pulse power generators, inverter type and pulsed direct current type were investigated. The sample temperature for inverter generator was higher than that for pulsed direct current generator in same die temperature ranging form 800 to 1400℃. The relative density increased with increasing of the sample temperature.
Pulsed electric current sintering (PECS) pulse waveform sample temperature relative density alumina
Khanh Quoc Dang Makoto Nanko Masakazu Kawahara Shinichi Takei
Department of Mechanical Engineering, Nagaoka University of Technology, Niigata, JAPAN SPS SYSTEX Inc., Kanagawa, JAPAN SINTERLAND Inc., Niigata, JAPAN
国际会议
10th International Symposium on Eco-Materials Processing and Design(第10届国际生态材料加工与设计研讨会)
西安
英文
101-104
2009-01-13(万方平台首次上网日期,不代表论文的发表时间)