会议专题

Transformations in Palladium Induced with Hydrogen:Scientific and Technological Aspects

There are summarized known facts about reverse and non-reverse structural transformatiorsinduced with hydrogen in palladium-hydrogen alloys: reverse stationary swelling of metal surface, nonreverse grains shift, and solitons, moving on metal surface. There is concluded that these effects must be taken in account during elaboration of exploitation technologies of palladium membranes for extra pure hydrogen production and hydrogen energy problems solving.

Palladium Hydrogen action Grains border Swelling Soliton

Goltsova M.V. Zhirov G.I. Goltsov V.A.

Donetsk National Technical University,58 Artema Str.,Donetsk83001,Ukraine