Preparation of Titanium-rich Material Ilmenite Concentrate by Reduction-rustion Process
Laboratory scale experiments were conducted to produce titanium-rich material from Panzhihua ilmenite. The results showed preoxidation with sodium salt additive especially for Na2B4O7 significantly advance the reduction of iron in Panzhihua ilmenite. Acceleration mechanism of preoxidation with Na2B4O7 has been studied here. The maximum metallization of iron 92% can be obtained under conditions of preoxidation at 850℃ for 30 min and subsequent reduction at 1100℃ for 150 min.The rusting separation technique to reduced ilmenite has been further studied, obtaining titanium-rich product with TiO2 over 82% and the recovery of TiO2 above 97%.
Ilmenite Reduction Rusting Titanium-rich material
Y. F. Guo X. W. Ma D. Huang G. H. Li H. G. Dong G. You G. Z. Qiu T. Jiang
School of Minerals Processing & Bioengineering, Central South University, changsha, China
国际会议
XXIV International Mineral Processing Congress(第24届国际矿物加工大会)
北京
英文
2228-2234
2008-09-24(万方平台首次上网日期,不代表论文的发表时间)