Study on New Technique for Advancing Recovery of Micro-sized Hematite by Magnetic Separation

For its surface features, micro-sized hematite is usually difficult to recover by magnetic separation; especially, the existing high gradient magnetic separator in industry can not utilize collecting matrix with thin silky rods for its property of being easily blocked; the lower size limit for recovery of micro-sized weak magnetic minerals is about 0.019mm, some even is 0.037mm. This paper introduces the application of the combined new technique of water-air joint discharging of concentrate and collecting matrix with different diameter silky rods in the field of recovery of micro-sized hematite by high gradient magnetic separator. The commercial test result for recovery of a certain hematite with size about -0.037mm shows that the recovery can be promoted by 16.81% with basically same concentrate grade.

Micro-size fraction Magnetic separation of hematite Collecting matrix Water-air joint discharging of ore

Y. H. Tang Y. B. Zhu J. Q. He Abubaker F. Spat

Guangdong Key Laboratory of Mineral Resource Development and Comprehensive Utilization,Guangzhou Res Department of Mining Engineering, AL-Fateh University, Libya Tarabulus Tripoli

国际会议

XXIV International Mineral Processing Congress(第24届国际矿物加工大会)

北京

英文

724-728

2008-09-24(万方平台首次上网日期,不代表论文的发表时间)