Structure and Properties of Wool Keratin Coated Cotton Fiber

In this study, wool keratin solution was firstly obtained by dissolving the wool fibers in the sodium hydroxide solution and peroxide solution, and then was used to treat the dialdehyde cellulose cotton fibers. The technical conditions of oxidized cotton fiber treated with keratin solution were discussed, as well as the structure and properties of treated oxidized cotton fibers. Results showed that the tensile properties of oxidized cotton fiber changed little before or after keratin treatment, while their weight changed a lot. Covalent group occurred between oxidized cotton fibers and keratin indicated by FTIR spectra.

wool keratin cotton oxidation Schiffs base

YANG Li UN Hong CHEN Yu-yue WANG Hao YANG Mei-gui

College of Material Engineering, Soochow University 178 East Ganjiang Road, Suzhou 215021, Jiangsu, P. R. China

国际会议

第六届中国国际丝绸会议暨第二届国际纺织高层论坛(The 6th China International Silk Conference and The 2nd International Textile Forum)

苏州

英文

395-398

2007-09-13(万方平台首次上网日期,不代表论文的发表时间)