HIP diffusion bonding of P/M titanium alloy Ti-6Al-4V and stainless steel 1Cr18Ni9Ti
The HIP diffusion bonding of P/M titanium alloy Ti-6Al-4V and stainless steel 1Cr18Ni9Ti using pure Ni as intermediate layer was studied.Bonding joint with complex bonding interface was obtained by HIPing pre-alloyed Ti-6Al-4V powders and stainless steel 1Cr18Ni9Ti in a vacuum canning.The joint strengths were examined and the characteristics of bonding joint were observed.The result shows that the maximized strength of HIP diffusion bonding between P/M titanium alloy Ti-6Al-4V and stainless steel 1Cr18Ni9Ti can be up to 388 MPa and the microstructure of bonding joint is acceptable.
Ti-6Al-4V 1Cr18Ni9Ti HIP diffusion bonding stainless steel titanium alloy powder metallurgy
LANG Ze-bao WANG Liang ZHANG Xu-hu
Aerospace Research Institute of Materials and Processing Technology,Beijing 100076,China