Microstructure and properties of p-type (Bi0.25Sb0.75)2Te3 fabricated by spark plasma sintering
P-type thermoelectric material (Bi0.25Sb0.75)2Te3 was sintered by spark plasma sintering(SPS) process in the temperature range of 320.420 .℃ The microstructures of sintered materials were found to be well aligned,particularly when sintered at lower sintering temperatures.The electrical conductivity of the material became larger as the sintering temperature increased.The Seebeck coefficient showed a general decreasing tendency with an increase in sintering temperature.In terms of the power factor,the optimum sintering temperature was found to be 380 for a maximum value of around ℃ 2.6 mW/K.
(Bi0.25Sb0.75)2Te3 thermoelectric material spark plasma sintering(SPS) sintering temperature
WANG Fu-qiang CHEN Hui WANG Zhong CHENG Yan CHU Ying ZHU Lei JIAN Xu-yu
Energy Materials and Technology Research Institute,General Research Institute for Nonferrous Metals,Beijing 100088,China
国际会议
2007年国际有色金属大会(International Conference of Nonfereous Materials 2007)(ICNFM)
长沙
英文
2007-11-28(万方平台首次上网日期,不代表论文的发表时间)