Mechanical and thermal properties of ceramic bonded carbonby using different carbon powders in degree of graphitization

  To adjust mechanical and thermal properties of SiC ceramic bonded carbon(SiC/CBC,30 vol%SiC)for desired applications,meso phase carbon powders heat-treated at different temperatures of 1 200℃,2 300 ℃and 2 500 ℃were used and compared.The results show that the SiC/CBC using the 1 200 ℃treated powder exhibits the highest strength of 220 Mpa and the lowest thermal conductivity of 90 W/mK,whereas the sample using the 2 500 ℃treated powder has the highest thermal conductivity of 166 W/mK and the lowest bending strength of 151 Mpa.The properties can be adjusted by changing the degree of graphitization.The effects of carbon powders on the interface between carbon particles and SiC layers were investigated.

Carbon ceramic composite Graphitization SPS,Mechanical property Thermal conductivity

Weiwu Chen Yoshinari Miyamoto

Joining and Welding Research Institute,Osaka University,11-1,Mihogaoka,Ibaraki,Osaka,Japan,567-0047; Joining and Welding Research Institute,Osaka University,11-1,Mihogaoka,Ibaraki,Osaka,Japan,567-0047;

国内会议

第十二届全国新型炭材料学术研讨会

长沙

英文

1-4

2015-11-05(万方平台首次上网日期,不代表论文的发表时间)