In-situ Investigation on the Pitting Corrosion Behavior of Friction Stir Welded Joint of AA2024 Aluminium Alloy
The surface corrosion behavior of an AA2024-T3 aluminium alloy sheet after friction stir welding was investigated by using an ”in-situ observation” method.SEM observations showed that the density and degree of the pitting corrosion in the shoulder active zone were slightly larger compared to the other regions on the top surface.The origins of the pitting corrosion were in the regions between the S phase particles and the adjacent aluminium base.The effect of Al-Cu-Fe-Mn-(Si) intermetallic compounds on the pitting corrosion was attributed to their high self-corrosion potential which induced the anodic dis-solution of the surrounding aluminium matrix.
A.Aluminium A.Intermetallics B.SEM C.Pitting corrosion C.Welding
Ju Kang Rui-dong Fu Guo-hong Luan Chun-lin Dong Miao He
College of Materials Science and Engineering,Yanshan University, Qinhuangdao, Hebei Prov.066004, PR State Key Laboratory of Metastable Materials Science and Technology, Qinhuangdao,Hebei Prov.066004, China FSW Center,Beijing FSW Technology Limited Company, Beijing 100024, PR China
国内会议
北京
英文
228-237
2012-10-18(万方平台首次上网日期,不代表论文的发表时间)