Modification of primary Mg2Si in Mg-5Si alloys with Y2O3
The Y2O3 addition to Mg-5Si alloys has a good modification effect on the primary Mg2Si.With 0.05% or 0.1% (mass fraction) Y2O3 additions,the primary Mg2Si begins to change from coarse dendritic shape (about 100 μm) into small polyhedral shape and therefore the alloys exhibits sub-modified microstructure.With 0.2% Y2O3 addition,most of the primary Mg2Si becomes polyhedral shape and its average size is only 25 μm or less.The Mg-5Si alloy exhibits modified microstructure.In addition,the experiments show that the reaction between Mg and Y2O3 cannot occur in the sintered Mg-6Y2O3 compact; however,the reaction among Mg,Si and Y2O3 can occur in the sintered Mg-5Si-6Y2O3 compact.Apart from the adsorption and poisoning manners,other mechanisms may exist in the modification of Y2O3 addition on the primary Mg2Si.
microstructure solidification Mg2Si Y2O3 Mg-5Si alloy
ZHENG Na WANG Hui-yuan ZHAO Feng GU Zhen-hua LI Dong JIANG Qi-chuan
Key Laboratory of Automobile Materials of Ministry of Education,Department of Materials Science and Engineering,Jilin University,Changchun 130025,China
国际会议
2007年国际有色金属大会(International Conference of Nonfereous Materials 2007)(ICNFM)
长沙
英文